The Properties of Uranium Containing Minor Additions of Aluminum or Zirconium (open access)

The Properties of Uranium Containing Minor Additions of Aluminum or Zirconium

This report discusses studies revealing the tensile properties, hot hardness, and heat treatment characteristics of uranium alloys with added aluminum or zirconium.
Date: July 16, 1956
Creator: Saller, Henry A.; Rough, Frank A. & Chubb, Walston
System: The UNT Digital Library
A PROPOSAL FOR A GENERALIZED CARD KEY PUNCH (open access)

A PROPOSAL FOR A GENERALIZED CARD KEY PUNCH

A key punch is discussed which would be useful in any automatic coding system requiring the initial input to be made via cards with 12 rows such as the standard IBM card. The proposed key punch consists of a keyboard connected to a punch and a electric typewriter so that if a character is struck, it is both punched in a single card column and typed on a sheet of paper. Each character key contains three characters which may be used in superscript, subscript, or main line position. (M.H.R.)
Date: July 16, 1956
Creator: Voorhees, E.A.
System: The UNT Digital Library
The Properties of Uranium Containing Minor Additions of Aluminum or Zirconium (open access)

The Properties of Uranium Containing Minor Additions of Aluminum or Zirconium

The tensile properties, hot hardness, and heattreatment characteristics of urarnium alloys containing up to 2.9 at.% aluminum or 4.0 at.% zirconium are described. The data shown that zirconium has a favorable effect upon the grain size, hardness, and tensile strength of uranium without materially affecting ductility. Additions of 3.8 at. % zirconium raised the tensile strength of uranium at room temperature fiom about 100,000 psi to about 200,000 psi, while the elongation in 2 in. increased from 14 to 22% and the grain size decreased from about 0.20 mm to less than O.01 mm. The data show that aluminum raises the yield strength, that it has very little effect on either the grain size, hardness, or tensile strength of uranium, and that it decreases ductility. The addition of 2.6 at.% aluminum decreased ihe roomtemperature ductility of ur-anium from l4 to 4%. (auth)
Date: July 16, 1956
Creator: Saller, H. A.; Rough, F. A. & Chubb, W.
System: The UNT Digital Library
Calculation of Residual Activity in APPR-1 Shielding Rings After Shutdown (open access)

Calculation of Residual Activity in APPR-1 Shielding Rings After Shutdown

None
Date: July 16, 1956
Creator: Fairbanks, F. B. & Morse, D. C.
System: The UNT Digital Library
HRP-BP: A MATHEMATICAL ANALYSIS OF THE HRT BLANKET PROCESSING PLANT (open access)

HRP-BP: A MATHEMATICAL ANALYSIS OF THE HRT BLANKET PROCESSING PLANT

None
Date: July 16, 1956
Creator: Carter, W. L.
System: The UNT Digital Library
EFFECT OF MELTING FAST CORE OF INTERNAL EXPONENTIAL EXPERIMENT (open access)

EFFECT OF MELTING FAST CORE OF INTERNAL EXPONENTIAL EXPERIMENT

None
Date: July 16, 1956
Creator: Hummell, Harry
System: The UNT Digital Library
Task I specifications for Purex feed (open access)

Task I specifications for Purex feed

None
Date: July 16, 1956
Creator: Browne, W. G.
System: The UNT Digital Library