A Coated Cast Iron Crucible for use with Eutectic Al-Si Alloy in the Temperature Range 595°-650°C (open access)

A Coated Cast Iron Crucible for use with Eutectic Al-Si Alloy in the Temperature Range 595°-650°C

The feasibility of the coated metal crucible as a container for eutectic Al-Si alloy has been proven by test. Small, enamel-coated cast iron pots has been proven by test. Small, enamel-coated cast iron pots have successfully withstood the chemically aggressive Al-Si alloy and the adverse influence of an oxidizing atmosphere for a period of 3 months at 725°C. A similarly coated castiron crucible containing 450 pounds of eutectic Al-Si alloy was successfully tested for 144 days in a jacketing operation conducted at 595°-650°C. Under the same conditions, the normal service life of clay-bonded graphite and silicon carbide crucibles rarely exceeds 45 days. The coating material is a commercially available enamel capable of withstanding temperatures up to 790°C (1450°F). It is readily applied to the surface of a variety of ferrous metals and alloys; however, best results are obtained with alloys low in chromium and nickel which also have a low thermal expansion coefficient.
Date: November 1957
Creator: Yaggee, F. L.
System: The UNT Digital Library