Uranium Oxide Slurry Pumping Experiments (open access)

Uranium Oxide Slurry Pumping Experiments

Abstract: Experiments on colloid milling and pumping show that uranium trioxide, when carefully dehydrated, can be dispersed in water to form a relatively stable slurry, suitable for a homogeneous slurry pile. At temperatures considerably below those of anticipated pile operation particle size growth occurs attended by increase in settling rate and decrease in viscosity. Theses properties of the slurries may be strongly affected by impurities present as well as by special operating conditions.
Date: September 15, 1944
Creator: Brandt, R. & Dean, G. R.
System: The UNT Digital Library
Electrolytic Production of Uranium from Solutions of its Tribromide in Fused Salts (open access)

Electrolytic Production of Uranium from Solutions of its Tribromide in Fused Salts

Abstract. the electrodeposition of uranium metal, in the form of tree-like deposits, from molten strontium halide baths is described. Under the best conditions studied, approximately 40% recovery is attained. Freedom from side-reactions of the reduced uranium with anode products and/or refractory materials, and high cathode current densities appear to be essential to the success of the process. the refining of uranium under similar conditions appears to occur quite readily, with approximately 50% current efficiency. The preparation of UI3 is also described.
Date: August 15, 1944
Creator: Webster, Richard A.
System: The UNT Digital Library
Sealing of Holes in Aluminum Sheet by Oxidation (open access)

Sealing of Holes in Aluminum Sheet by Oxidation

Aluminum oxide occupies a larger volume than the aluminum it contains would fill as metal, consequently, the assumption has been made that holes in metallic aluminum would close by a sufficient amount of oxidation. Therefore, we were asked to investigate the rate of plug formation under conditions to be expected in the pile. For the latter we were requested to approach the pile conditions as nearly as we could by employing the Chicago cyclotron. It seems to us that the problem divides itself into two separate questions: (1) under what conditions may holes be expected to close? (2) if holes do close how much corrosion of uranium may be expected before the closure becomes impervious to water vapor? In this report only the first question is considered. The experiments and theory coupled with the data collected by other workers on the project definitely define the limits within which pores in the aluminum cans may be expected to close by an oxidation process. Under the most favorable conditions only small holes may be sealed in this manner. In the large majority of the cases the holes not only fail to close but become larger.
Date: July 15, 1944
Creator: Anderson, S. & Goldowski, N.
System: The UNT Digital Library
The Flow of a Compressible Fluid Past a Circular Arc Profile (open access)

The Flow of a Compressible Fluid Past a Circular Arc Profile

"The Ackeret iteration process is utilized to obtain higher approximations than that of Prandtl and Glauert for the flow of a compressible fluid past a circular arc profile. The procedure is to expand the velocity potential in a power series of the camber coefficient. The first two terms of the development correspond to the Prandtl-Glauert approximation and yield the well-known correction to the circulation about the profile" (p. 385).
Date: July 15, 1944
Creator: Kaplan, Carl
System: The UNT Digital Library
Effects of Small Angles of Sweep and Moderate Amounts of Dihedral on Stalling and Lateral Characteristics of a Wing-Fuselage Combination Equipped With Partial- and Full-Span Double Slotted Flaps (open access)

Effects of Small Angles of Sweep and Moderate Amounts of Dihedral on Stalling and Lateral Characteristics of a Wing-Fuselage Combination Equipped With Partial- and Full-Span Double Slotted Flaps

"Tests of a wing-fuselage combinations incorporating NACA 65-series airfoil sections were conducted in the NACA 19-foot pressure tunnel. The investigation included the tests with flaps neutral and with partial- and full-span double slotted flaps deflected to determine the effects of (1) variations of wing sweep between -4 degrees and 8 degrees on stalling and lateral stability and control characteristics and (2) variations of dihedral between 0 degree and 6.75 degrees on lateral stability characteristics" (p. 467).
Date: April 15, 1944
Creator: Teplitz, Jerome
System: The UNT Digital Library
Fission Product Poisoning in a Pile (open access)

Fission Product Poisoning in a Pile

Abstract. The effect of the neutron flux on the relative importance of different fission product poisons is discussed. The general expression for the poising of a fission product is given with the various equations for special cases of interest. The formulae are applied to the problem of finding the poisoning due to fission products at the end of one day in a pile operating with a flux of 4 x 10(14) neutrons/cm(2)/soc. These results are summarized in the table on page 12. Appendix I contains a revised list of cross sections x yields for all stable isotopes. Such a list was first given by Wheeler in CP-889. Appendix II contains a list of radioactive fission products with half lives greater than one day with data about yields, parents, gaseous ancestors, and numbers of neutrons.
Date: December 15, 1944
Creator: Way, Katharine, 1903-
System: The UNT Digital Library